Dongguan International Technology Transfer Center, 124 Dongbao Road, Dongcheng District, Dongguan, China
Request a quote
Mixing Screw for Color and Additive Dispersion
Screws for Injection Molding

Mixing Screw for Color and Additive Dispersion

Adds a dispersive or distributive section to solve color streaks, specks and temperature variation.

Made to your drawing, sample or part number

Machined to your barrel dimensions and screw geometry — no catalogue constraints. Single replacement part or production batch.

Quoted to confirmed specs

Engineering review Monday to Saturday. Send the machine model, screw diameter and resin — the reply carries price, material grade and lead time.

Email engineering

No drawing on file? Send a photo of the worn part and the machine model — we work the geometry back and confirm it with you before machining.

Details

Specification & application

A mixing screw adds a dispersive or distributive element at the metering end. It is not a different way of melting — it is a way of homogenizing what has already melted, which is why it is usually specified on top of a three-zone or barrier profile rather than instead of one.

Mixing elements

ElementMixing typeBest for
PinsDistributiveSimple color and regrind blending; easy to clean
Maddock / slotted flightDispersiveMasterbatch agglomerates, filled compounds
Saucer or pineappleDistributive with some shearGeneral homogenizing at moderate output
Static mixer in the nozzleDistributiveWhen the screw cannot be changed but mixing must improve

Geometry

ParameterTypical rangeNote
Mixer lengthUsually 3 to 8 diametersLonger mixing costs pressure and adds shear heat
Number of pins or slotsSet by the dispersion problemMore elements help dispersion but raise pressure drop
Channel depth in the mixerShallower than meteringNeeds enough pressure to push melt through the restriction
Surface treatmentSame as the rest of the screwMixers wear at the flight tips first

When to specify one

  • Color streaks that survive a full purge and a screw removal.
  • Masterbatch that leaves visible specks, indicating agglomerates are not being broken up.
  • Weight variation between shots that cannot be traced to the check ring or the process.
  • Regrind blends where the two components have very different melt viscosities.

When not to

If the problem is unmelted resin rather than unmixed resin, a mixer will not help — it will just add shear heat to solids that never melted in the first place. Fix the melting length first.

Related

Other components in this range

View category

Need this part matched to your press?

Send the machine model and the resin. We confirm geometry, material and surface treatment before quoting.

Mixing Screw for Color and Additive Dispersion Quoted to confirmed specs